Alteration of soda silicate glasses by organic pollutants in museums : mechanisms and kinetics
TitelAlteration of soda silicate glasses by organic pollutants in museums : mechanisms and kinetics
Verantwoordelijke(n)
Bron Journal of Non-Crystalline Solids ; nr. 355 (2009), pagina's 1479–1488
Materiaalartikel
SamenvattingThe role of the organic pollutants formic acid, acetic acid and formaldehyde in the alteration of unstable
soda silicate glasses is examined through SIMS depth profiling of replica glass aged in polluted and nonpolluted
atmospheres under ambient conditions. The effect of different controlled atmospheres is compared
to the polluted atmosphere encountered in museum storage. The results show that formic acid
rather than formaldehyde is responsible for the increased alteration in the National Museums of Scotland
glass collection. Formic acid caused sodium formate crystals to form at the glass surface and increased the
leaching of alkali. Acid pollutants increased both the alteration depth and the amount of sodium
extracted from the altered layer, which fell to a concentration 1 at.%, compared to 4–5 at.% in the
non-acidic atmospheres. The research highlights the gap existing between alteration models obtained
from controlled laboratory experiments, predicting an eventual slowing down of the alteration, and
the reaction process taking place in real environments (as found in museums), where the environmental
fluctuations maintain a roughly linear progression of the alteration. The storage of unstable glasses in
wooden cabinets or showcases emitting organic pollutants must be avoided and glasses should be kept
in stable environmental conditions.
Keywords±
Corrosion; Ion exchange; Archaeology; Secondary ion mass spectrocopy; Optical microscopy; Raman spectroscopy; Alkali silicates; Soda–lime–silica
soda silicate glasses is examined through SIMS depth profiling of replica glass aged in polluted and nonpolluted
atmospheres under ambient conditions. The effect of different controlled atmospheres is compared
to the polluted atmosphere encountered in museum storage. The results show that formic acid
rather than formaldehyde is responsible for the increased alteration in the National Museums of Scotland
glass collection. Formic acid caused sodium formate crystals to form at the glass surface and increased the
leaching of alkali. Acid pollutants increased both the alteration depth and the amount of sodium
extracted from the altered layer, which fell to a concentration 1 at.%, compared to 4–5 at.% in the
non-acidic atmospheres. The research highlights the gap existing between alteration models obtained
from controlled laboratory experiments, predicting an eventual slowing down of the alteration, and
the reaction process taking place in real environments (as found in museums), where the environmental
fluctuations maintain a roughly linear progression of the alteration. The storage of unstable glasses in
wooden cabinets or showcases emitting organic pollutants must be avoided and glasses should be kept
in stable environmental conditions.